Excellent adhesion on built plate, it allows an easy detachment and quick cleaning cycle with isopropilic alchool.
Safe with no unpleasant odors, an UV post curing process is required.
Compatible with disinfectants and autoclave. Under medical certification process, it is only suitable for test.
Relative density | ca 1.1 - 1.2 | ||
Viscosity mPas | 450 - 850 | ||
Layer thickness 0.05 mm | LCD | LCD Mono | DLP |
Base exp layer 6 - 8 | 60 | 50 | 45 |
Normal exp. layer | 6 | 4 | 3 |
Reference temperature | 25 C° | ||
UV 405 nm uniform light source | min. 45 Watt |
Above 25 C° reduce the layers by 0.5 sec. every 3 degrees in up, while increase them by 1 sec. for every 2 degrees to down
All 3D printing resins are heat sensitive, therefore the best prints are achieved in heated environments and in hot seasons.
During the cold months put the printer in a warm place and preheat the resin up to 28 C° for at least 20 min. If necessary, also preheat the building plate and shake well the bottle before the use, if possible with a roller agitator. Remove and filter the resin from the vat at the end of each print.
Store the resins between 10 and 21 C° and protected from direct light